Sunday, 6 April 2014

Folder


I did my sons CRKT folder today, took about 30 minutes.

I used the Edge Pro at 17 Degrees.

Progression was:

Atoma 140 to reprofile
EP 220
Chosera 400
Shapton Glass 1,000
Shapton Glass 2, 000
Chosera 3,000
Shapton Pro 5,000
Chosera 10,000

Lots of water and some dish detergent on the stones.

thanks for looking

Peter